MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Alclad Aluminum 3004-O
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes: Composition for AA 3004 (not Alclad 3004 specifically).
Composition information provided by the Aluminum Association and is not for design.

Key Words: Alclad 3004-O; Alclad 3004-O; Al3004-O
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.72 g/cc0.0983 lb/in³For AA3004 (Not Alclad)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 179 MPa26000 psiAA; Typical
 145 - 195 MPa
@Thickness 0.152 - 12.7 mm
21000 - 28300 psi
@Thickness 0.00600 - 0.499 in
 150 - 200 MPa
@Thickness 12.7 - 76.2 mm
21800 - 29000 psi
@Thickness 0.500 - 3.00 in
Tensile Strength, Yield 68.9 MPa10000 psiAA; Typical
 >= 55.0 MPa
@Thickness 0.152 - 12.7 mm
>= 7980 psi
@Thickness 0.00600 - 0.499 in
 >= 59.0 MPa
@Thickness 12.7 - 76.2 mm
>= 8560 psi
@Thickness 0.500 - 3.00 in
Elongation at Break  10 - 18 %
@Thickness 0.152 - 12.7 mm
10 - 18 %
@Thickness 0.00600 - 0.499 in
 16 %
@Thickness 12.7 - 76.2 mm
16 %
@Thickness 0.500 - 3.00 in
 20 %
@Thickness 1.59 mm
20 %
@Thickness 0.0625 in
AA; Typical
 25 %
@Diameter 12.7 mm
25 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 68.9 GPa10000 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Shear Strength 110 MPa16000 psiAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 95.5 - 98.2 %95.5 - 98.2 %As remainder
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.80 - 1.3 %0.80 - 1.3 %
Manganese, Mn 1.0 - 1.5 %1.0 - 1.5 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.30 %<= 0.30 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 3004-O
Aluminum 3003-O
Alclad Aluminum 3003-O
Aluminum 5052-O
Alclad Aluminum 3003-H112

MA3004AO / 8991

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.