MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toray TORAYCON™ PBT Resin 1101GM55BL Polybutylene Terephthalate (PBT), 55% Glass Fiber
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled

Material Notes: Reinforced, high stiffness, GF55%. PBT+P-GF55.

General Toraycon™ Notes: TORAYCON™ PBT (polybutylene terephthalate) is a polyester-based thermoplastic engineering plastic with excellent electrical properties and chemical resistance. PBT resin is produced from the primary starting materials 1,4-butanediol and terephthalic acid and is a linear thermoplastic saturated polyester resin with ester bonds in the main chain. Unique features can be easily provided by compounding various additives, glass fibers, flame retardants, and utilizing solubilizing techniques. Furthermore, it is easy to add any color. The product is used in a large number of applications spanning several fields, including electrical and electronic devices, connectors and capacitor casing, automotive electronics, OA equipment, building materials, and industrial machinery parts.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.79 g/cc0.0647 lb/in³ISO 1183
Water Absorption 0.070 %
@Time 86400 sec
0.070 %
@Time 24.0 hour
In 23°C water; ISO 62
Linear Mold Shrinkage, Flow 0.0025 cm/cm0.0025 in/in80x80x3mmt; Toray Method
Linear Mold Shrinkage, Transverse 0.0053 cm/cm0.0053 in/in80x80x3mmt; Toray Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ISO 2039-2
Tensile Strength 165 MPa23900 psiISO 527-1,2
Elongation at Break 1.5 %1.5 %ISO 527-1,2
Flexural Strength 265 MPa38400 psiISO 178
Flexural Modulus 17.0 GPa2470 ksiISO 178
Charpy Impact Unnotched 6.80 J/cm²32.4 ft-lb/in²ISO 179
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²V-Notched; ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 23.0 kV/mm584 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 26.0 µm/m-°C
@Temperature -30.0 - 100 °C
14.4 µin/in-°F
@Temperature -22.0 - 212 °F
ISO 11359-2
CTE, linear, Transverse to Flow 32.0 µm/m-°C17.8 µin/in-°FISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 221 °C430 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1,2
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9077 / 248767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.