MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BCC Products BC 4553 Polyester Styling Paste
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: BC4553 is designed for instant buildup and repair of plastic surfaces and models. Recommended for use on SMC and FRP parts, vacuum form molds and a variety of surfaces. When cured BC4553 produces a hard, strong, chip resistant, tack-free surface. Area to be filled should be clean and dry, free from dust, oil and release agents. It is advisable to scarify the area prior to application. May be applied at any reasonable thickness by spreading or splining. Do not work with more material than can be applied in 5 minutes. Material mixed with cream hardener should not be returned to original can. After final cure material may be scraped, sanded, filed, drilled, taped or machined to a featheredge. Available in Ultra-white, gray, pine and mahogany

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Cure Time 20.0 - 60.0 min
@Temperature 24.0 °C
0.333 - 1.00 hour
@Temperature 75.2 °F
Pot Life 5.0 - 10 min
@Temperature 24.0 °C
5.0 - 10 min
@Temperature 75.2 °F
1lb mass
Shelf Life 6.00 Month6.00 Monthin tightly closed container
 
Descriptive Properties
Mix Ratio100:1 or 100:2 resin/hardener
Mixed Viscosity, BrookfieldThixotropic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten Carbide, WC
Industeel FORA 360 BC 360 HB Wear Resistant Steel
Goodfellow Hot Pressed Boron Carbide B4C
Boron Carbide, B4C
BCC Products BC 4544 Polyester Carvable Wood Filler

PBCC002 / 107229

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.