MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Acetal Copolymer, Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.40 - 1.58 g/cc0.0506 - 0.0571 lb/in³Average value: 1.46 g/cc Grade Count:61
Filler Content 10.0 - 40.0 %10.0 - 40.0 %Average value: 18.8 % Grade Count:17
Water Absorption 0.200 - 1.00 %0.200 - 1.00 %Average value: 0.351 % Grade Count:11
Moisture Absorption at Equilibrium 0.100 - 0.800 %0.100 - 0.800 %Average value: 0.250 % Grade Count:10
Additive Loading 10.0 - 20.0 %10.0 - 20.0 %Average value: 16.3 % Grade Count:8
Linear Mold Shrinkage 0.000500 - 0.0234 cm/cm0.000500 - 0.0234 in/inAverage value: 0.00460 cm/cm Grade Count:52
Linear Mold Shrinkage, Transverse 0.00600 - 0.0300 cm/cm0.00600 - 0.0300 in/inAverage value: 0.0114 cm/cm Grade Count:10
Melt Flow 2.00 - 12.0 g/10 min2.00 - 12.0 g/10 minAverage value: 5.51 g/10 min Grade Count:18
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 85.0 - 95.085.0 - 95.0Average value: 90.5 Grade Count:6
Tensile Strength, Ultimate 65.0 - 217 MPa9430 - 31500 psiAverage value: 111 MPa Grade Count:55
Tensile Strength, Yield 51.0 - 86.0 MPa7400 - 12500 psiAverage value: 71.5 MPa Grade Count:5
Elongation at Break 0.600 - 25.0 %0.600 - 25.0 %Average value: 2.77 % Grade Count:58
Elongation at Yield 1.00 - 10.0 %1.00 - 10.0 %Average value: 4.00 % Grade Count:5
Modulus of Elasticity 2.40 - 23.4 GPa348 - 3400 ksiAverage value: 11.7 GPa Grade Count:46
Flexural Yield Strength 44.8 - 304 MPa6500 - 44100 psiAverage value: 156 MPa Grade Count:55
Flexural Modulus 2.40 - 17.2 GPa348 - 2500 ksiAverage value: 10.1 GPa Grade Count:57
Flexural Strain at Break 1.10 - 2.90 %1.10 - 2.90 %Average value: 1.75 % Grade Count:4
Izod Impact, Notched 0.320 - 4.50 J/cm0.599 - 8.43 ft-lb/inAverage value: 0.696 J/cm Grade Count:36
Izod Impact, Unnotched 2.14 - 6.94 J/cm4.00 - 13.0 ft-lb/inAverage value: 3.85 J/cm Grade Count:27
Charpy Impact Unnotched 1.20 J/cm² - NB5.71 ft-lb/in² - NBAverage value: 3.96 J/cm² Grade Count:9
Charpy Impact, Notched 0.300 - 0.730 J/cm²1.43 - 3.47 ft-lb/in²Average value: 0.477 J/cm² Grade Count:20
Coefficient of Friction 0.140 - 0.3900.140 - 0.390Average value: 0.276 Grade Count:5
K (wear) Factor 5.00 - 10000 x 10-8 mm³/N-M2.48 - 4960 x 10-10 in³-min/ft-lb-hrAverage value: 2650 x 10-8 mm³/N-M Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00 - 2.00e+7 ohm-cm1.00 - 2.00e+7 ohm-cmAverage value: 686000 ohm-cm Grade Count:44
Surface Resistance 0.800 - 1.00e+7 ohm0.800 - 1.00e+7 ohmAverage value: 372000 ohm Grade Count:31
Static Decay 0.500 - 2.00 sec0.500 - 2.00 secAverage value: 1.63 sec Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 100 µm/m-°C5.56 - 55.6 µin/in-°FAverage value: 36.8 µm/m-°C Grade Count:19
CTE, linear, Transverse to Flow 80.0 - 110 µm/m-°C44.4 - 61.1 µin/in-°FAverage value: 95.0 µm/m-°C Grade Count:8
Thermal Conductivity 0.400 - 0.450 W/m-K2.78 - 3.12 BTU-in/hr-ft²-°FAverage value: 0.417 W/m-K Grade Count:3
Melting Point 160 - 172 °C320 - 342 °FAverage value: 166 °C Grade Count:12
Maximum Service Temperature, Air 100 - 120 °C212 - 248 °FAverage value: 110 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 160 - 171 °C320 - 340 °FAverage value: 164 °C Grade Count:16
Deflection Temperature at 1.8 MPa (264 psi) 94.0 - 166 °C201 - 330 °FAverage value: 156 °C Grade Count:53
Vicat Softening Point 151 - 165 °C304 - 329 °FAverage value: 159 °C Grade Count:7
Flammability, UL94 HBHBGrade Count:40
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 230 °C350 - 446 °FAverage value: 196 °C Grade Count:5
Nozzle Temperature 175 - 220 °C347 - 428 °FAverage value: 195 °C Grade Count:6
Melt Temperature 170 - 230 °C338 - 446 °FAverage value: 197 °C Grade Count:33
Mold Temperature 60.0 - 120 °C140 - 248 °FAverage value: 92.7 °C Grade Count:38
Drying Temperature 75.0 - 121 °C167 - 250 °FAverage value: 110 °C Grade Count:33
Moisture Content 0.150 %0.150 %Average value: 0.150 % Grade Count:21
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:21
Injection Pressure 30.0 - 118 MPa4350 - 17100 psiAverage value: 83.0 MPa Grade Count:30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, PTFE Filled
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced

O1257 / 77846

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.