MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALTECH® ABS A 2020/100 GF20 ABS, 20% Glass Fibers Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled

Material Notes: Base Polymer: Acrylonitrile Butadiene Styrene Copolymer

Filler/Additive System: 20% glass fibers

Special Features: Injection molding grade, processing stabilized

Application Area: Various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Time 86400 sec
0.0020 - 0.0040 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Time 86400 sec
0.0040 - 0.0060 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 5.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 125 MPa18100 psiH358/10; ISO 2039-1
Elongation at Break 1.6 %1.6 %ISO 527
Tensile Modulus 5.80 GPa841 ksiISO 527
Flexural Strength 105 MPa15200 psiISO 178
Flexural Modulus 5.80 GPa841 ksiISO 178
Charpy Impact Unnotched 1.80 J/cm²8.57 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FISO 75-1/-2
Vicat Softening Point 103 °C217 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 260 °C428 - 500 °FInjection molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °FInjection molding
Drying Temperature  80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 80.0 °C
@Time 10800 - 21600 sec
176 °F
@Time 3.00 - 6.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerAcrylonitrile Butadiene Styrene Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omni Plastics OmniTech™ ABS GR20 ABS, 20% Glass Reinforced
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
INEOS Styrolution Absolac® 30GF20 ABS, 20% Glass Filled
Chase Plastics CP Pryme® A220G ABS Molding Resin, 20% Glass Fiber Reinforced
Chase Plastics CP Pryme® A120 ABS, 20% Glass Fiber Reinforced

PALBIS8622 / 242681

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.