MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Carmel Olefins CARMELCLEAR™ MT 74 A Specialty Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: CARMELCLEAR™ MT 74 A is a modified polypropylene for injection molding of high impact transparent articles. It exhibits excellent impact resistance at low and ambient temperatures, very good transparency combined with good flexibility and low stress-whitening. It contains anti-static additives.

APPLICATIONS

CARMELCLEAR™ MT 74 A is suitable for clear ice cream boxes, flexible lids with tight closure properties, see-through delicate tool packaging, and clear “freezer to microwave” food boxes. It is frequently used as an impact modifier in blends with random copolymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 230 °C
22 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.650 GPa94.3 ksiASTM D790
Izod Impact, Notched  0.700 J/cm
@Temperature >=-20.0 °C
1.31 ft-lb/in
@Temperature >=-4.00 °F
ASTM D256
 5.00 J/cm
@Temperature >=23.0 °C
9.37 ft-lb/in
@Temperature >=73.4 °F
ASTM D256
 
Optical PropertiesMetricEnglishComments
Haze 32 %
@Thickness 1.60 mm
32 %
@Thickness 0.0630 in
plaque; ASTM D1003
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AdvanSix Capran® NyLid™ OMBS-100M Nylon 6/EVOH Lidding Film

PCARM038 / 79776

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.