MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Arkema Rilsan® BZM 8 O TL PA11-GF8
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11 with 10% Glass Fiber Filler

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
 1.07 g/cc0.0387 lb/in³Cond.; ISO 1183
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 235 °C
18 g/10 min
@Load 11.0 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 73
@Time 15.0 sec
73
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength at Break 56.0 MPa8120 psiCond.; ISO 527-1/-2
Elongation at Break 26 %26 %Cond.; ISO 527-1/-2
Tensile Modulus 2.30 GPa334 ksiCond.; ISO 527-1/-2
Charpy Impact Unnotched  8.80 J/cm²
@Temperature -30.0 °C
41.9 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 9.30 J/cm²
@Temperature 23.0 °C
44.3 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C33.3 µin/in-°FDry; ISO 11359-1/-2
Melting Point 189 °C372 °F10°C/min; Dry; ISO 11357-1/-3
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
Oxygen Index 22 %22 %Dry; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
Hold Pressure 19.0 MPa2760 psiInjection Molding; ISO 294
 
Descriptive Properties
%Bio-Based97ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsInjection Molding
Release agentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsan® BSR 30 PA11-CF30
Arkema Rilsan® BUM 30 O PA11-GB30
Arkema Rilsan® Clear G300 HI PA
Arkema Rilsan® Clear G850 Rnew® PA
Arkema Rilsan® BZM 30 O TL PA11-GF30

PARKF911 / 193648

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.