MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 685 HB Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber - UL94 HB
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled

Material Notes: The RTP 680 HB are carbon fiber reinforced ABS. These materials offer a good combination of physical properties, stiffness and the ability to be fabricated to close dimensional tolerances.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D 792
Water Absorption 0.16 %
@Time 86400 sec
0.16 %
@Time 24.0 hour
ASTM D 570
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm
@Thickness 3.20 mm
0.00050 - 0.0015 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D 785
Tensile Strength at Break 124 MPa18000 psiASTM D 638
Elongation at Break 1.2 %1.2 %ASTM D 638
Tensile Modulus 18.6 GPa2700 ksiASTM D 638
Flexural Strength 186 MPa27000 psiASTM D 790
Flexural Modulus 17.2 GPa2500 ksiASTM D 790
Izod Impact, Notched 0.641 J/cm
@Thickness 3.20 mm
1.20 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 3.20 J/cm
@Thickness 3.20 mm
6.00 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1e+05<= 1e+05ASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C235 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 238 °C400 - 460 °F
Mold Temperature 62.8 - 85.0 °C145 - 185 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
ASTM A678 Steel, grade C, plate thickness 38 - 51 mm
ASTM A678 Steel, grade C, plate thickness 19 - 38 mm
ASTM A678 Steel, grade C
RTP Company RTP 285 D SI 2 Nylon 6/12 (PA), Carbon Fiber - Silicone Lubricated

PQZWA2202 / 91023

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.