MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Nylon, Amorphous Transparent Alloy
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon, Amorphous Transparent Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 - 1.40 g/cc0.0368 - 0.0506 lb/in³Average value: 1.11 g/cc Grade Count:7
 0.900 - 0.900 g/cc
@Temperature >=250 °C
0.0325 - 0.0325 lb/in³
@Temperature >=482 °F
Average value: 0.900 g/cc Grade Count:2
Viscosity Number 100 - 200 cm³/g1.00 - 2.00 dl/gAverage value: 153 cm³/g Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80.0 - 89.080.0 - 89.0Average value: 82.8 Grade Count:4
Ball Indentation Hardness 108 - 200 MPa15700 - 29000 psiAverage value: 132 MPa Grade Count:4
Tensile Strength, Ultimate 50.0 - 140 MPa7250 - 20300 psiAverage value: 72.5 MPa Grade Count:4
Tensile Strength, Yield 60.0 - 98.0 MPa8700 - 14200 psiAverage value: 72.5 MPa Grade Count:6
Elongation at Break 2.10 - 150 %2.10 - 150 %Average value: 88.1 % Grade Count:7
 >= 50.0 %
@Temperature 80.0 - 80.0 °C
>= 50.0 %
@Temperature 176 - 176 °F
Average value: 50.0 % Grade Count:1
Elongation at Yield 3.00 - 9.00 %3.00 - 9.00 %Average value: 7.56 % Grade Count:6
Modulus of Elasticity 1.40 - 10.0 GPa203 - 1450 ksiAverage value: 3.12 GPa Grade Count:6
 1.27 - 1.27 GPa
@Temperature 80.0 - 80.0 °C
184 - 184 ksi
@Temperature 176 - 176 °F
Average value: 1.27 GPa Grade Count:1
Flexural Yield Strength 50.0 - 190 MPa7250 - 27600 psiAverage value: 87.1 MPa Grade Count:4
Flexural Modulus 1.65 - 12.0 GPa239 - 1740 ksiAverage value: 4.05 GPa Grade Count:5
Charpy Impact Unnotched 7.70 J/cm² - NB36.6 ft-lb/in² - NBAverage value: 7.70 J/cm² Grade Count:5
 5.90 J/cm² - NB
@Temperature -30.0 - 0.000 °C
28.1 ft-lb/in² - NB
@Temperature -22.0 - 32.0 °F
Average value: 6.45 J/cm² Grade Count:5
Charpy Impact, Notched 0.900 - 1.80 J/cm²4.28 - 8.57 ft-lb/in²Average value: 1.35 J/cm² Grade Count:6
 0.600 - 1.70 J/cm²
@Temperature -30.0 - 0.000 °C
2.86 - 8.09 ft-lb/in²
@Temperature -22.0 - 32.0 °F
Average value: 1.24 J/cm² Grade Count:6
Tensile Creep Modulus, 1 hour 1300 - 10000 MPa189000 - 1.45e+6 psiAverage value: 4230 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 700 - 8300 MPa102000 - 1.20e+6 psiAverage value: 3230 MPa Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 - 1.00e+17 ohm-cm1.00e+15 - 1.00e+17 ohm-cmAverage value: 5.05e+16 ohm-cm Grade Count:6
Surface Resistance 1.00e+13 - 1.00e+15 ohm1.00e+13 - 1.00e+15 ohmAverage value: 5.05e+14 ohm Grade Count:6
Dielectric Constant 3.00 - 5.003.00 - 5.00Average value: 3.56 Grade Count:6
Dielectric Strength 21.0 - 35.0 kV/mm533 - 889 kV/inAverage value: 27.5 kV/mm Grade Count:4
Dissipation Factor 0.0115 - 0.03250.0115 - 0.0325Average value: 0.0217 Grade Count:6
Comparative Tracking Index 575 - 600 V575 - 600 VAverage value: 589 V Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 32.0 - 90.0 µm/m-°C17.8 - 50.0 µin/in-°FAverage value: 67.0 µm/m-°C Grade Count:6
CTE, linear, Transverse to Flow 30.0 - 90.0 µm/m-°C16.7 - 50.0 µin/in-°FAverage value: 75.0 µm/m-°C Grade Count:4
Melting Point 250 °C482 °FAverage value: 250 °C Grade Count:3
Maximum Service Temperature, Air 100 °C212 °FAverage value: 100 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 100 - 150 °C212 - 302 °FAverage value: 123 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 93.0 - 140 °C199 - 284 °FAverage value: 110 °C Grade Count:7
Vicat Softening Point 105 - 158 °C221 - 316 °FAverage value: 134 °C Grade Count:6
Glass Transition Temp, Tg 108 - 150 °C226 - 302 °FAverage value: 136 °C Grade Count:5
Flammability, UL94 HB - V-2HB - V-2Grade Count:5
Glow Wire Test 850 °C1560 °FAverage value: 850 °C Grade Count:3
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 85.0 - 90.0 %85.0 - 90.0 %Average value: 89.2 % Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Trogamid® CX9701 Transparent Nylon
Evonik Trogamid® CX7323 Transparent Nylon
Overview of materials for Nylon 6-3
Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

O2680 / 78080

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.