MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Arkema Rilsamid® AZM 23 BLACK T6LD PA12-GF23
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³Cond.; ISO 1183
 1.18 g/cc0.0426 lb/in³ISO 1183
Water Absorption 1.3 %1.3 %Dry; Sim. to ISO 62
Moisture Absorption 0.500 %0.500 %Dry; Sim. to ISO 62
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 235 °C
13 g/10 min
@Load 11.0 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psiDry; ISO 527-1/-2
 100 MPa14500 psiCond.; ISO 527-1/-2
Tensile Strength, Yield 101 MPa14600 psiDry; ISO 527-1/-2
 105 MPa15200 psiCond.; ISO 527-1/-2
Elongation at Break 5.0 %5.0 %Dry; ISO 527-1/-2
 5.2 %5.2 %Cond.; ISO 527-1/-2
Elongation at Yield 3.0 %3.0 %Dry; ISO 527-1/-2
 3.5 %3.5 %Cond.; ISO 527-1/-2
Tensile Modulus 5.07 GPa735 ksiCond.; ISO 527-1/-2
 5.50 GPa798 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  6.60 J/cm²
@Temperature -30.0 °C
31.4 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 6.60 J/cm²
@Temperature 23.0 °C
31.4 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 7.70 J/cm²
@Temperature 23.0 °C
36.6 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eU
 8.30 J/cm²
@Temperature -30.0 °C
39.5 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 5.0
@Frequency 100 Hz
5.0
@Frequency 100 Hz
Dry; IEC 60250
Dissipation Factor  0.0364
@Frequency 1e+6 Hz
0.0364
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.117
@Frequency 100 Hz
0.117
@Frequency 100 Hz
Dry; IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C33.3 µin/in-°FDry; ISO 11359-1/-2
Melting Point 179 °C354 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 173 °C343 °FDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °FDry; ISO 75-1/-2
Vicat Softening Point 165 °C329 °F50°C/h 50N; Dry; ISO 306
Decomposition Temperature 222 °C432 °F1% wt. loss, TGA, in air
 223 °C433 °F1% wt. loss, TGA, in nitrogen
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
Hold Pressure 16.0 MPa2320 psiInjection Molding; ISO 294
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsInjection Molding
Release agentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® BG-30 EC PA6-GF30
EMS-Grivory Grilamid® 1SBVX-30H LDS black PA1010-GF30
Arkema Rilsamid® AZM 30 BLACK T6LD PA12-GF30
BASF Capron® 8200 HS BK-102 Nylon 6 (Dry)
E-Polymers EFLEX® S1030 General

PARKF864 / 193612

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.