Description: As a non-oil-extended rubber, thermoplastic elastomer SBS rubber 792 is polystyrene(S)-polybutadiene(B)-polystyrene(S) triblock copolymer with linear molecular structure and medium molecular weight. The styrene content of SBS polymer 792 is 40%. Application: Adhesives/Asphalt modification/Compounding Formula: Shoe adhesive (Parts by mass) SBS(YH792): 100 Coumarone Resin: 70-90 Terpene Resin:40-60 Antioxygen: 1 Gasoline and Ethyl Acetate: 450-500 Information provided by BEC Materials, LLC |