MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Acetal Copolymer, Silicone Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Silicone Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.29 - 1.62 g/cc0.0466 - 0.0585 lb/in³Average value: 1.42 g/cc Grade Count:23
Filler Content 2.00 - 4.00 %2.00 - 4.00 %Average value: 2.67 % Grade Count:3
Water Absorption 0.0500 - 0.700 %0.0500 - 0.700 %Average value: 0.241 % Grade Count:10
Additive Loading 2.00 %2.00 %Average value: 2.00 % Grade Count:3
Linear Mold Shrinkage 0.00400 - 0.0350 cm/cm0.00400 - 0.0350 in/inAverage value: 0.0203 cm/cm Grade Count:21
Linear Mold Shrinkage, Transverse 0.0140 - 0.0210 cm/cm0.0140 - 0.0210 in/inAverage value: 0.0183 cm/cm Grade Count:3
Melt Flow 8.00 - 49.0 g/10 min8.00 - 49.0 g/10 minAverage value: 16.4 g/10 min Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 75.0 - 83.075.0 - 83.0Average value: 79.3 Grade Count:3
Hardness, Rockwell R 79.0 - 82.079.0 - 82.0Average value: 80.0 Grade Count:3
Tensile Strength, Ultimate 41.4 - 110 MPa6000 - 16000 psiAverage value: 57.2 MPa Grade Count:14
Tensile Strength, Yield 41.4 - 56.0 MPa6000 - 8120 psiAverage value: 49.8 MPa Grade Count:7
Elongation at Break 2.50 - 90.0 %2.50 - 90.0 %Average value: 30.6 % Grade Count:20
Elongation at Yield 8.50 - 12.0 %8.50 - 12.0 %Average value: 10.5 % Grade Count:5
Modulus of Elasticity 2.25 - 2.90 GPa326 - 420 ksiAverage value: 2.56 GPa Grade Count:10
Flexural Yield Strength 57.0 - 172 MPa8270 - 24900 psiAverage value: 79.4 MPa Grade Count:21
Flexural Modulus 2.07 - 7.60 GPa300 - 1100 ksiAverage value: 2.61 GPa Grade Count:21
Izod Impact, Notched 0.440 - 0.961 J/cm0.824 - 1.80 ft-lb/inAverage value: 0.717 J/cm Grade Count:13
 0.500 - 0.500 J/cm
@Temperature -29.0 - -29.0 °C
0.937 - 0.937 ft-lb/in
@Temperature -20.2 - -20.2 °F
Average value: 0.500 J/cm Grade Count:1
Izod Impact, Unnotched 11.7 - 5340 J/cm22.0 - 10000 ft-lb/inAverage value: 11.7 J/cm Grade Count:6
Charpy Impact Unnotched 7.50 - 15.0 J/cm²35.7 - 71.4 ft-lb/in²Average value: 11.3 J/cm² Grade Count:3
Charpy Impact, Notched 0.500 - 1.00 J/cm²2.38 - 4.76 ft-lb/in²Average value: 0.739 J/cm² Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm1.00e+14 - 1.00e+16 ohm-cmAverage value: 4.76e+15 ohm-cm Grade Count:11
Surface Resistance 1.00e+14 - 1.00e+16 ohm1.00e+14 - 1.00e+16 ohmAverage value: 7.30e+15 ohm Grade Count:7
Dielectric Strength 17.7 - 19.7 kV/mm450 - 500 kV/inAverage value: 18.2 kV/mm Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 - 234 µm/m-°C50.0 - 130 µin/in-°FAverage value: 130 µm/m-°C Grade Count:9
Melting Point 165 - 170 °C329 - 338 °FAverage value: 167 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 150 - 166 °C302 - 331 °FAverage value: 161 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 145 °C176 - 293 °FAverage value: 103 °C Grade Count:18
Flammability, UL94 HBHBGrade Count:13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 160 - 230 °C320 - 446 °FAverage value: 197 °C Grade Count:13
Mold Temperature 48.9 - 120 °C120 - 248 °FAverage value: 86.6 °C Grade Count:13
Drying Temperature 82.2 - 121 °C180 - 250 °FAverage value: 109 °C Grade Count:12
Moisture Content 0.150 %0.150 %Average value: 0.150 % Grade Count:6
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:6
Injection Pressure 30.0 - 103 MPa4350 - 15000 psiAverage value: 77.1 MPa Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acetal Copolymer, Impact Modified
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, Mineral Filled
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced

O1256 / 77845

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.