MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips DRISCOPLEX® 6400 Oil and Gas Gathering HDPE PIPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: DriscoPlex® 6300 Pipe meets or exceeds:
ASTM D2513
Title 49, Code of Federal Regulations, Part 192
API 15LE
ASTM D3350, cell classification PE445574C
PPI TR-4 designation PE4710 I
ron Pipe Size OD (IPS), ¾” – 36”
40’ and 50’ Joints / Coils available thru 6” / Solid Black

DriscoPlex® 6300 Pipe for:
Class 3, Class 4 and Federally Regulated:
• Oil & Gas Gathering
• Coal Bed Methane
• Landfill Methane

Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³black; ASTM D1505
Carbon Black Loading >= 2.00 %>= 2.00 %UV Stabilizer; ASTM D3350
High Load Melt Index 0.0800 g/10 min
@Load 21.6 kg,
Temperature 190 °C
0.0800 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 500 hour>= 500 hourASTM F1473
Hardness, Shore D 62.062.0ASTM D2240
Tensile Strength, Yield >= 24.1 MPa>= 3500 psiASTM D638 Type IV
Elongation at Break >= 800 %>= 800 %2 in / min., Type IV Bar; ASTM D638
Modulus of Elasticity >= 1.21 GPa>= 175 ksiASTM D638
Flexural Modulus >= 0.827 GPa>= 120 ksi2% Secant – 16:1 span: depth. 0.5 in / min.; ASTM D790
Hydrostatic Design Basis  6.89 MPa
@Temperature 60.0 °C
1000 psi
@Temperature 140 °F
ASTM D2837
 11.0 MPa
@Temperature 23.0 °C
1600 psi
@Temperature 73.4 °F
ASTM D2837
 
Thermal PropertiesMetricEnglishComments
CTE, linear 180 µm/m-°C100 µin/in-°FASTM D696
Vicat Softening Point 124 °C256 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEVC8806 / 323309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.