Dielectric Conformal Coatings for Electronics Cytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, instrumentation (industrial and military), missiles, spacecraft, fire and smoke detectors as well as coatings for electronic components, coils and transformers. And no small reason why -- all of the coatings described have been specifically formulated as dielectric insulating coatings to provide the user the ultimate protection available for his electronic assemblies; be it environmental (dirt, dust, humidity, fungus, temperature extremes, etc) or electrical insulation of conductors. These coatings are not designed for use as floor coatings or other general purpose uses; they have been produced under essentially "clean-room" conditions using raw materials with a minimum of ionizable impurities which would detract from their insulating qualities.
Cytec (Conap) CE-1175 Conathane® Polyurethane Dielectric Conformal Coating
- Single Component
- Passes Thermal Shock Test (MIL-I-46058C)
- Non-Nutrient Fungus Resistance (MIL-I-46058C)
- Passes Flexibility Test (1/8" Mandrel Bend) (MIL-I-46058C)
- Good Chemical and Solvent Resistance
- Solvent Evaporation Cure
Cure Type: Solvent Evaporation Information provided by Cytec, subsequently acquired by Elantas. |