MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Envalior Stanyl® SC50 PA46-GF30 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Flame Retarded + Glass Fiber Reinforced

Material Notes: 30% Glass Reinforced, Flame Retardant, Halogen free and free of red phosphorous

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³dry; ISO 1183
Moisture Absorption 2.10 %2.10 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 100 MPa14500 psicond; ISO 527-1/-2
 140 MPa20300 psidry; ISO 527-1/-2
Elongation at Break 1.7 %1.7 %dry; ISO 527-1/-2
 2.5 %2.5 %cond; ISO 527-1/-2
Tensile Modulus 8.00 GPa1160 ksicond; ISO 527-1/-2
 12.5 GPa1810 ksidry; ISO 527-1/-2
Flexural Modulus 8.00 GPa1160 ksicond; ISO 178
 12.5 GPa1810 ksidry; ISO 178
Charpy Impact Unnotched  3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eU
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmcond; IEC 60093
 >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmdry; IEC 60093
Dielectric Strength 20.0 kV/mm508 kV/incond; IEC 60243-1
 30.0 kV/mm762 kV/indry; IEC 60243-1
Comparative Tracking Index 425 V425 Vdry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°Fdry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C25.0 µin/in-°Fdry; ISO 11359-1/-2
Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 275 °C527 °Fdry; ISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
dry; IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TS250F6D PA46-GF30 FR, Conditioned, 30% Glass Filled, Flame Retardant, Heat Stabilized
Envalior Stanyl® TW275F6 PA46-GF30, Dry, 30% Glass Filled, Heat Stabilized
Envalior Stanyl® TW275F6 PA46-GF30, Conditioned, 30% Glass Filled, Heat Stabilized
Envalior Stanyl® TW241F6 PA46-GF30, Dry, 30% Glass Filled, Heat Stabilized
Envalior Stanyl® TW241F6 PA46-GF30, Conditioned, 30% Glass Filled, Heat Stabilized

PDSM9923 / 161544

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.