MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Blasch Ceramics NITRON Nitride bonded SiC
Categories: Ceramic; Carbide

Material Notes: Features:
  • Properties suit many severe operating conditions
  • Good wear and abrasion
  • Resists wetting by non-ferrous metals
  • High mechanical strength
  • Excellent Thermal shock resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Porosity 16 %16 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0414 GPa6.00 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.68 µm/m-°C
@Temperature 20.0 °C
2.60 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 14.0 - 20.0 W/m-K97.2 - 139 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Si3N4 21 %21 %
SiC 70 %70 %
SiO2 + Si2ON2 8.9 %8.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5%
Ceradyne Ceralloy® 7712 Al2O3-SiC
Silicon Carbide, Alpha SiC
Silicon Carbide, CVD
Silicon Carbide, sublimed

CBLASCH0 / 647

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.