MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

AISI 5132 Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 5000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Key Words: B.S. 530 A 32, B.S. 530 H 32, UNS G51320
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 174 - 212174 - 212annealed and cold drawn.
Hardness, Knoop 215215Converted from Brinell
Hardness, Rockwell B 9191Converted from Brinell
Hardness, Rockwell C 1212Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 202202Converted from Brinell
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Calculated
Machinability 70 %70 %annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000210 ohm-cm
@Temperature 20.0 °C
0.0000210 ohm-cm
@Temperature 68.0 °F
hardened and tempered specimen; unknown specimen
 0.0000259 ohm-cm
@Temperature 100 °C
0.0000259 ohm-cm
@Temperature 212 °F
hardened and tempered specimen; unknown specimen
 0.0000330 ohm-cm
@Temperature 200 °C
0.0000330 ohm-cm
@Temperature 392 °F
hardened and tempered specimen; unknown specimen
 0.0000517 ohm-cm
@Temperature 400 °C
0.0000517 ohm-cm
@Temperature 752 °F
hardened and tempered specimen; unknown specimen
 0.0000778 ohm-cm
@Temperature 600 °C
0.0000778 ohm-cm
@Temperature 1110 °F
hardened and tempered specimen; unknown specimen
 0.0000934 ohm-cm
@Temperature 700 °C
0.0000934 ohm-cm
@Temperature 1290 °F
hardened and tempered specimen; unknown specimen
 0.0001106 ohm-cm
@Temperature 800 °C
0.0001106 ohm-cm
@Temperature 1470 °F
hardened and tempered specimen; unknown specimen
 0.0001145 ohm-cm
@Temperature 900 °C
0.0001145 ohm-cm
@Temperature 1650 °F
hardened and tempered specimen; unknown specimen
 0.0001177 ohm-cm
@Temperature 1000 °C
0.0001177 ohm-cm
@Temperature 1830 °F
hardened and tempered specimen; unknown specimen
 0.0001205 ohm-cm
@Temperature 1100 °C
0.0001205 ohm-cm
@Temperature 2010 °F
hardened and tempered specimen; unknown specimen
 0.000123 ohm-cm
@Temperature 1200 °C
0.000123 ohm-cm
@Temperature 2190 °F
hardened and tempered specimen; unknown specimen
 0.0001251 ohm-cm
@Temperature 1300 °C
0.0001251 ohm-cm
@Temperature 2370 °F
hardened and tempered specimen; unknown specimen
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  0.494 J/g-°C
@Temperature >=100 °C
0.118 BTU/lb-°F
@Temperature >=212 °F
annealed.
 0.502 J/g-°C
@Temperature 150 - 200 °C
0.120 BTU/lb-°F
@Temperature 302 - 392 °F
Thermal Conductivity  44.3 W/m-K
@Temperature 200 °C
307 BTU-in/hr-ft²-°F
@Temperature 392 °F
Tested when annealed.
 46.5 W/m-K
@Temperature 100 °C
323 BTU-in/hr-ft²-°F
@Temperature 212 °F
Tested when annealed.
 48.6 W/m-K
@Temperature 0.000 °C
337 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
Tested when annealed.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.30 - 0.35 %0.30 - 0.35 %
Chromium, Cr 0.75 - 1.0 %0.75 - 1.0 %
Iron, Fe 97.475 - 98.2 %97.475 - 98.2 %As remainder
Manganese, Mn 0.60 - 0.80 %0.60 - 0.80 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 5135 Steel
AISI 5120H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 775°C (1430°F), 150°C (300°F) temper
AISI 5130 Steel
AISI 5132H Steel
AISI 50B40 Steel

M513BA / 8061

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.