MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Capron® 8253 Impact Modified Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions. Copolymerization results in improved dry as molded toughness and increased flexibility to meet higher impact performance compared to conventional unreinforced homopolymers. Good nylon thermal and chemical properties are maintained along with good strength and stiffness retention.

Capron 8253 is generally recommended for applications such as plugs, receptacles, flexible connector covers, weed trimmer components, clips, fasteners, flanges, key housings as well as many flexible tubing applications. ASTM Callout PA254 + PA0270 B40410.

Data provided by Allied Signal.

Processing: Max. water content 0.2%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 240-270 degC (464-518 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 10 degC (50 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO data
Water Absorption 1.5 %1.5 %24 hrs; ISO data
Moisture Absorption at Equilibrium 2.3 %2.3 %50% RH; 23°C; ISO data
Water Absorption at Saturation 8.1 %8.1 %in water; 23°C; ISO data
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inISO data
 0.012 cm/cm0.012 in/inASTM data MD
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 60.0 MPa8700 psiASTM data at 5 mm/min.
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; Same value from ASTM and ISO test.
Elongation at Break >= 50 %>= 50 %Nominal
 >= 100 %>= 100 %Nominal
Elongation at Yield 4.0 %4.0 %ISO Value at 50 mm/min.
 4.0 %4.0 %ASTM Value at 50 mm/min.
Tensile Modulus 2.53 GPa367 ksisame value from ASTM and ISO test.
Flexural Yield Strength 90.0 MPa13100 psiASTM Data
Flexural Modulus 2.165 GPa314.0 ksiISO Value
 2.21 GPa321 ksiASTM Value
Poissons Ratio 0.350.35ISO data
Shear Modulus 0.900 GPa131 ksicalculated
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO Data
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO data
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmISO data
Comparative Tracking Index 600 V600 VISO data
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 88.0 µm/m-°C
@Temperature 20.0 °C
48.9 µin/in-°F
@Temperature 68.0 °F
ISO data
CTE, linear, Transverse to Flow 93.0 µm/m-°C
@Temperature 20.0 °C
51.7 µin/in-°F
@Temperature 68.0 °F
ISO data
Melting Point 220 °C428 °FASTM and ISO test
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FISO data
 168 °C334 °FASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C133 °FISO data
 60.0 °C140 °FASTM Data
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 °C536 °FSee Materials Notes
Mold Temperature 70.0 °C158 °FSee Materials Notes
Drying Temperature 85.0 °C185 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
BASF Capron® BU50I Ultratough Nylon 6 (Dry)
Lucite International Diakon® TD542 Toughened Acrylic Compound
BASF Ultramid® 8202 HS PA6 (Conditioned)
BASF Ultramid® 1000-2 NF2001 PA66 (Dry)

PALC69 / 23863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.