Unitika AXG-1500-300 Conditioned
Categories:
Polymer
;
Thermoplastic
;
Polyarylate
Material Notes:
Characteristics:
Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistances
Favorable rigidity and dimensional accuracy
Information provided by Unitika Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
112
MPa
16200
psi
ASTM D638
Elongation at Break
6.0 %
6.0 %
ASTM D638
Flexural Strength
181
MPa
26300
psi
ASTM D790
Flexural Modulus
6.30
GPa
914
ksi
ASTM D790
Izod Impact, Notched
1.03
J/cm
@Thickness 3.17 mm
1.93
ft-lb/in
@Thickness 0.125 in
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+12
ohm-cm
1.00e+12
ohm-cm
ASTM D257
Dielectric Constant
3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength
30.0
kV/mm
762
kV/in
ASTM D149
Dissipation Factor
0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance
60
sec
60
sec
ASTM D495
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
210
-
230
°C
410
-
446
°F
Middle Barrel Temperature
240
-
260
°C
464
-
500
°F
Front Barrel Temperature
250
-
270
°C
482
-
518
°F
Nozzle Temperature
250
-
270
°C
482
-
518
°F
Mold Temperature
80.0
-
120
°C
176
-
248
°F
actual surface temp
Drying Temperature
100
°C
212
°F
Dry Time
10.0
-
24.0
hour
10.0
-
24.0
hour
Back Pressure
0.490
-
1.47
MPa
71.1
-
213
psi
gage pressure
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Unitika AX-1500 Conditioned
Unitika C300VN
Westlake Plastics Ardel® Polyarylate
Unitika PT-3020
Unitika LM-8503-10
PUNITIK894 / 177914
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.