MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral/Graphite Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 - 2.06 g/cc0.0592 - 0.0744 lb/in³Average value: 1.79 g/cc Grade Count:11
Water Absorption 0.0300 - 0.0500 %0.0300 - 0.0500 %Average value: 0.0423 % Grade Count:11
Linear Mold Shrinkage 0.00173 - 0.00540 cm/cm0.00173 - 0.00540 in/inAverage value: 0.00315 cm/cm Grade Count:11
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 58.0 - 85.058.0 - 85.0Average value: 63.5 Grade Count:6
Tensile Strength, Ultimate 31.0 - 89.0 MPa4500 - 12900 psiAverage value: 45.9 MPa Grade Count:11
Elongation at Break 0.236 - 0.580 %0.236 - 0.580 %Average value: 0.388 % Grade Count:11
Modulus of Elasticity 10.3 - 29.0 GPa1490 - 4210 ksiAverage value: 15.6 GPa Grade Count:11
Flexural Yield Strength 55.0 - 163 MPa7980 - 23600 psiAverage value: 78.7 MPa Grade Count:11
Flexural Modulus 10.0 - 26.0 GPa1450 - 3770 ksiAverage value: 13.6 GPa Grade Count:11
Compressive Yield Strength 117 - 269 MPa17000 - 39000 psiAverage value: 153 MPa Grade Count:11
Izod Impact, Notched 0.156 - 0.174 J/cm0.292 - 0.326 ft-lb/inAverage value: 0.163 J/cm Grade Count:8
Charpy Impact Unnotched 0.310 - 0.960 J/cm²1.48 - 4.57 ft-lb/in²Average value: 0.543 J/cm² Grade Count:3
Charpy Impact, Notched 0.130 - 0.260 J/cm²0.619 - 1.24 ft-lb/in²Average value: 0.170 J/cm² Grade Count:10
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 - 25.0 µm/m-°C7.78 - 13.9 µin/in-°FAverage value: 18.3 µm/m-°C Grade Count:4
 32.0 - 38.0 µm/m-°C
@Temperature 40.0 - 130 °C
17.8 - 21.1 µin/in-°F
@Temperature 104 - 266 °F
Average value: 34.0 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 30.0 - 32.0 µm/m-°C16.7 - 17.8 µin/in-°FAverage value: 31.0 µm/m-°C Grade Count:3
Thermal Conductivity 1.22 - 1.94 W/m-K
@Temperature 100 - 100 °C
8.47 - 13.5 BTU-in/hr-ft²-°F
@Temperature 212 - 212 °F
Average value: 1.58 W/m-K Grade Count:2
Maximum Service Temperature, Air 200 - 257 °C392 - 495 °FAverage value: 223 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 159 - 222 °C318 - 432 °FAverage value: 187 °C Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
Overview of materials for Phenolic, Resole, Glass Fiber Filled
Overview of materials for Phenolic, Resole, Mineral/Flock Filled
Overview of materials for Phenolic; Unreinforced; Molded

O2724 / 78094

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.