MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 151-60 Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags.

Features:

  • Excellent flex fatigue resistance
  • Excellent Ozone Resistance

Product Notes: Values are for injection molded plaques, side gated.
102 mm x 152 mm x 2 mm

Information provided by Advanced Elastomer Systems.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 58585 seconds; ASTM D2240
Tensile Strength at Break 2.40 MPa348 psiAcross flow; ASTM D412
Tensile Stress at Strain 1.20 MPa
@Strain 100 %
174 psi
@Strain 100 %
across flow; ASTM D412
Elongation at Break 350 %350 %Across flow; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 26 %26 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 232 °C351 - 450 °F
Drying Temperature 82.0 °C180 °FDesiccant Dryer
Dry Time 3 hour3 hourDesiccant Dryer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 121-80M300 Thermoplastic Rubber
ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant
ExxonMobil Santoprene® 121-65W233 Thermoplastic Elastomer
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber

PADW150 / 22868

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.