MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Encom Polymers EnLon 601E Nylon 6, Extrusion Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Product Description: High Viscosity Extrusion Grade recommended for all types of extrusion including profile, film, and extrusion coating

Appearance: Black, Natural or Colors

Processing Methods: Extrusion, Blow Molding

Applications: Automotive, Material Handling, Industrial

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 70.0 MPa10200 psiASTM D638
Elongation at Break 140 %140 %ASTM D638
Izod Impact, Notched 0.530 J/cm0.993 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 266 - 277 °C510 - 530 °F
Middle Barrel Temperature 271 - 282 °C520 - 540 °F
Front Barrel Temperature 277 - 288 °C530 - 550 °F
Melt Temperature 288 - 302 °C550 - 575 °F
Head Temperature 550 - 575 °C1020 - 1070 °F
Drying Temperature 82.2 °C180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 <= 4.00 hour<= 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM022 / 266036

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.