MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman DuraGrip™ DGR 6040 NCHT Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: DuraGrip® DGR 6040NCHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with improved surface tack that produces superior grip qualities. DGR 6040NCHT, will bond to olefinics, and is easily colored. DuraGrip® DGR 6040NCHT is not hygroscopic and under normal conditions does not require drying.

Information provided by Advanced Polymer Alloys

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D471; ISO 2781
Viscosity 127000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
127000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040Time of 5 seconds; ASTM D2240; ISO 48
Tensile Strength, Ultimate 4.96 MPa720 psiASTM D412; ISO 37
Elongation at Break 751 %751 %ASTM D412; ISO 37
100% Modulus 1.21 MPa
@Strain 100 %
175 psi
@Strain 100 %
ASTM D412; ISO 37
 
Processing PropertiesMetricEnglishComments
Processing Temperature 216 °C420 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)
A. Schulman DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE)
A. Schulman DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE)
Borealis Daplen™ AK4504 TPO Compound
Borealis Daplen™ EF267AI Polypropylene TPO Compound

PAPA034 / 24101

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.