MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Boron Phosphide, BP, Low Temperature Form
Categories: Ceramic; Phosphide/Pnictide; Other Engineering Material; Semiconductor

Key Words: Pnictide; Semiconductor
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.90 g/cc0.105 lb/in³
a Lattice Constant 4.538 Å4.538 Å
Molecular Weight 41.785 g/mol41.785 g/mol
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 3700037000N/mm²
 
Electrical PropertiesMetricEnglishComments
Band Gap 2.1 eV2.1 eVApproximate
Electron Mobility, cm²/V-s 500500
Hole Mobility, cm²/V-s 7070
 
Thermal PropertiesMetricEnglishComments
Melting Point 2527 °C4581 °FApproximate
Debye Temperature 707 °C1300 °FApproximate
 
Descriptive Properties
ColorRed
Crystal StructureCubicSphalerite Structure - Space Group F(-4)3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Boron Phosphide, BP, High Temperature Form
Cadmium Polonide, CdPo
Cadmium Germanium Arsenide, CdGeAs2
Cadmium Gallium Telluride, CdGa2Te4
Cadmium Gallium Sulfide, CdGa2S4

DSEM20 / 2935

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.