MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChenGuang FH209 Fluoro-rubber Compounds
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Properties:
  • Outstanding H-temperature resistance.
  • Excellent resistance to fuel, oil, acid and chemicals.
  • Good resistance to gas penetration and radiation.
  • Besides, with all the properties of general rubber.
  • Outstanding physical, electrical and mechanical properties.
  • Can work in harsh, thermal, chemical, and UV environments where general rubber can not
Applications:
  • Extensively used in aerospace/aviation, automobile, petroleum and chemical, mechanical industry, and construction, communication and concrete industry, etc.
  • Mainly used as sealents resisting H-temperature, fuel, oil, etc., and as erosion-protection material, to make O-ring ,oil, etc., diaphragm, gaskets, rubber bowl and valve core, etc.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60 - 7060 - 70
Tensile Strength at Break >= 14.0 MPa>= 2030 psi
 <= 35.0 MPa
@Treatment Temp. 250 °C,
Time 86400 sec
<= 5080 psi
@Treatment Temp. 482 °F,
Time 24.0 hour
after aging
Elongation at Break >= 200 %>= 200 %
 <= 30 %
@Treatment Temp. 250 °C,
Time 86400 sec
<= 30 %
@Treatment Temp. 482 °F,
Time 24.0 hour
after aging
Compression Set <= 60 %
@Temperature 200 °C,
Time 86400 sec
<= 60 %
@Temperature 392 °F,
Time 24.0 hour
compression ratio 30%
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -30.0 °C<= -22.0 °F
 
Descriptive Properties
Heat Resistance<175°CLong Time
 <200°C20 ~30 hr
 <250°CShort Time ( ~ 5 hr)
Weight Increasing<6%in 1# jet fuel, 20oC, 24hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU013 / 255612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.