  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Elantas Conathane® CE-1164 (Conap) Polyurethane Dielectric Conformal Coating
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes:
Dielectric Conformal Coatings for Electronics
Cytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, instrumentation (industrial and military), missiles, spacecraft, fire and smoke detectors as well as coatings for electronic components, coils and transformers. And no small reason why -- all of the coatings described have been specifically formulated as dielectric insulating coatings to provide the user the ultimate protection available for his electronic assemblies; be it environmental (dirt, dust, humidity, fungus, temperature extremes, etc) or electrical insulation of conductors. These coatings are not designed for use as floor coatings or other general purpose uses; they have been produced under essentially "clean-room" conditions using raw materials with a minimum of ionizable impurities which would detract from their insulating qualities.

Cytec (Conap) CE-1164 Conathane® Polyurethane Dielectric Conformal Coating
  • Single Component
  • Passes Thermal Shock Test (MIL-I-46058C)
  • Non-Nutrient Fungus Resistance (MIL-I-46058C)
  • Passes Flexibility Test (1/8" Mandrel Bend) (MIL-I-46058C)
  • Very Good Chemical and Solvent Resistance
  • Moisture Cure (must have a minimum of 30% relative humidity to fully cure)
Cure Type: Moisture

Information provided by Cytec, subsequently acquired by Elantas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 50 %50 %
Viscosity 150 cP
@Temperature 25.0 °C
150 cP
@Temperature 77.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 4.50e+12 ohm-cm4.50e+12 ohm-cmInsulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity)
 2.50e+13 ohm-cm2.50e+13 ohm-cmInitial Insulation Resistance (50% Relative Humidity)
 1.30e+10 ohm-cm
@Temperature 65.0 °C
1.30e+10 ohm-cm
@Temperature 149 °F
Insulation Resistance During 10th day Cycling (95% Relative Humidity)
Dielectric Constant 2.72.7ASTM D150
Dielectric Strength 138 kV/mm3500 kV/inASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 54.4 °C130 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Flash Point 12.8 °C55.0 °F(TCC)
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 60.0 °C
4.00 hour
@Temperature 140 °F
 10080 min
@Temperature 25.0 °C
168.0 hour
@Temperature 77.0 °F
Tack-Free Time 20.0 - 30.0 min
@Temperature 25.0 °C
0.333 - 0.500 hour
@Temperature 77.0 °F
Shelf Life 12.0 Month12.0 MonthShelf Life Time at 25°C in original, unopened containers.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Taiyo America PSR-9000 FXT Series Liquid Photoimageable Solder Mask
Lord Adhesives Metech 7600A Cermet Multilayer Dielectric Composition
Dow XIAMETER® PMCPPMX-200 5CS Silicone Fluid
Dow 3-4130 DIELECTRIC GEL KIT
Dielectric TTR

PCYTEC01 / 29233

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.