MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company ESD 187 Polypropylene (PP), Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Carbon Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D 792
Additive Loading 40 %40 %Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0025 cm/cm
@Thickness 3.20 mm
0.00050 - 0.0025 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.4 MPa7170 psiASTM D 638
Elongation at Break 0.70 %0.70 %ASTM D 638
Tensile Modulus 14.5 GPa2100 ksiASTM D 638
Flexural Strength 27.6 MPa4000 psiASTM D 790
Flexural Modulus 11.0 GPa1600 ksiASTM D 790
Izod Impact, Notched 0.481 J/cm
@Thickness 3.20 mm
0.900 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 1.12 J/cm
@Thickness 3.20 mm
2.10 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  48 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
48 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 50 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
50 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 50 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
50 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 52 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
52 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 52 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
52 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 53 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
53 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 108 °C227 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 - 232 °C375 - 450 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 2561 FR UV Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - UV Stabilized
RTP Company EMI 2562 UV BLACK Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
RTP Company EMI 362 UV BLACK Polycarbonate (PC); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized

PQZQA40627 / 239947

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.