MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Angst+Pfister APSOplast® PPSU High-performance plastic
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: These PPSU semi-finished products offer better impact resistance and chemical resistance than PEI and PSU. PPSU also has excellent resistance to hydrolysis on the basis of the number of steam autoclave cycles before failure. This material has a practically unlimited superheated steam sterilizability. In addition, the raw material used to make PPSU semi-finished products meets the requirements of Class VI of the USP Standards and is thus a very popular material for the medical technology and pharmaceutical industries, for use in sterilization trays, handles of dental and surgical instructions, orthopedic test implants, and fluid technology couplings and fittings.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³DIN EN ISO 1183-1
Water Absorption  0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
DIN EN ISO 62
 0.65 %
@Time 346000 sec
0.65 %
@Time 96.0 hour
DIN EN ISO 62
Moisture Absorption 0.600 %0.600 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 143 MPa20700 psiDIN EN ISO 2039-1
Tensile Strength, Yield 77.0 MPa11200 psiDIN EN ISO 527
Elongation at Break 30 %30 %DIN EN ISO 527
Modulus of Elasticity 2.50 GPa363 ksiDIN EN ISO 527
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.44
@Frequency 50 Hz
3.44
@Frequency 50 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm381 kV/inIEC 60243
Comparative Tracking Index 100 V100 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
30.6 µin/in-°F
@Temperature 73.4 - 140 °F
Maximum Service Temperature, Air 180 °C356 °Flong term
 210 °C410 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FDIN EN ISO 75 / A
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP053 / 250551

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.