MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AdvanSix Capran® 980 Heat Stabilized Nylon Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: Description: Capran® 980 is a clear (low haze level), heat-stabilized cast film produced from modified nylon 6 resin. Capran® 980 has excellent heat stability and resistance to pinholing. It can be used at temperatures up to 390°F (199°C) for typical composite cure cycle times.

Applications: Capran® 980 is recommended as bagging film for advanced composite fabrication and other high temperature applications where dimensional stability, adherence to sealant tapes and uniform film gauge are essential.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0410 lb/in³Yield Density
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 110 MPa16000 psiASTM D882
Tensile Strength, Yield 34.0 MPa4930 psiASTM D882
Elongation at Break 375 %375 %ASTM D882
Tear Strength Test 4545grams/mil; ASTM D1922
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 - 220 °C424 - 428 °Fcrystalline melting point; Hot Stage Microscope
Shrinkage <= 2.0 %
@Temperature 149 °C,
Time 1800 sec
<= 2.0 %
@Temperature 300 °F,
Time 0.500 hour
ASTM D1204

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ArcelorMittal Dual Phase 980 LCE Y700 Very High Strength Cold Rolled Steel
ArcelorMittal Dual Phase 980 LCE Y600 Very High Strength Cold Rolled Steel
ArcelorMittal Dual Phase 780 Very High Strength Hot Rolled Steel
Polyram PlusTek PB140 Nylon 6, Injection Molding
Polyram PlusTek PB145 Nylon 6, Injection Molding

PALC019 / 23779

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.