MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Capron® 8253 Impact Modified Nylon 6 (Conditioned)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions. Copolymerization results in improved dry as molded toughness and increased flexibility to meet higher impact performance compared to conventional unreinforced homopolymers. Good nylon thermal and chemical properties are maintained along with good strength and stiffness retention.

Capron 8253 is generally recommended for applications such as plugs, receptacles, flexible connector covers, weed trimmer components, clips, fasteners, flanges, key housings as well as many flexible tubing applications. ASTM Callout PA254 + PA0270 B40410.

Data provided by Allied Signal.

Processing: Max. water content 0.2%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 240-270 degC (464-518 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 10 degC (50 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³(Dry)
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM Data MD (Dry)
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO Data (Dry)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 60.0 MPa8700 psiASTM data at 5 mm/min.
Tensile Strength, Yield 30.0 MPa4350 psiASTM value at 50 mm/min.
 32.0 MPa4640 psiISO value at 50 mm/min.
Elongation at Break >= 50 %>= 50 %Nominal
 >= 100 %>= 100 %Nominal
Elongation at Yield 14 %14 %ISO Value at 50 mm/min.
 15 %15 %ASTM Value at 50 mm/min.
Tensile Modulus 0.730 GPa106 ksisame value from ASTM and ISO test.
Flexural Yield Strength 30.0 MPa4350 psiASTM Data
Flexural Modulus 0.670 GPa97.2 ksiASTM Data
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F(Dry)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 °C536 °FSee Materials Notes
Mold Temperature 70.0 °C158 °FSee Materials Notes
Drying Temperature 85.0 °C185 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)
BASF Ultramid® 8202C HS PA6 (Conditioned)
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8253 HS PA6 (Dry)
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry)

PALC68 / 23862

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.