MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arya Sasol LFI 2125A Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description: LFI2125A is a low density polyethylene, with a medium level of anti-block and slip agent (Erucamide). This grade offers good optical properties, low energy consumption during processing, adequate COF level and excellent draw down. LFI2125A has been manufactured under SABTEC licensed technology.

Application: Blown film extrusion, packaging film for food and goods, general lamination film

Forms: Pellets

Attribute: Good toughness, high speed converting without sticking, good optical properties, suitable when ultimate down gauging is required

Additives: Antioxidant: Yes; Antiblock: Yes; Slip Agent: Yes

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ISO 1183
Thickness 20.0 - 50.0 microns0.787 - 1.97 mil
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.0 MPa1890 psiISO 527-1,3
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiISO 527-1,3
Film Elongation at Break, MD >= 100 %>= 100 %ISO 527-1,3
Film Elongation at Break, TD >= 500 %>= 500 %ISO 527-1,3
Modulus of Elasticity 0.180 GPa26.1 ksiTD; ISO 527-1,3
 0.190 GPa27.6 ksiMD; ISO 527-1,3
Coefficient of Friction 0.200.20ASTM D1894
Tear Strength 25.0 kN/m143 pliTD; ISO 6383-2
 70.0 kN/m399 pliMD; ISO 6383-2
Dart Drop Total Energy 23.0 J/cm0.0431 ft-lb/milASTM D4272
Film Tensile Strength at Break, MD 30.0 MPa4350 psiISO 527-1,3
Film Tensile Strength at Break, TD 19.0 MPa2760 psiISO 527-1,3
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM D1003 A
Gloss 60 %60 %[GU], 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 190 °C338 - 374 °FExtruder temperature profile
Blow-up Ratio (BUR) 2.0 - 3.02.0 - 3.0
 
Descriptive Properties
Blocking<5 gASTM D3354
Clarity30 mVSABTEC method
Re-blocking0 gSABTEC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARYA002 / 250456

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.