MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% glass fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Glass Fiber Filled

Material Notes: 40% glass fiber, high melt flow for injection molding

AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK)designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemical resistance expected of PEEK while maintaining excellent elevated temperature properties.

The price and performance of this resin will expand the opportunities for PEEK resins especially in the area of metal replacement for corrosion control.

- Natural: AvaSpire® AV-750 GF40 NT

Markets/Uses: Aircraft / Mechanical & Structural Applications / Electrical Connectors; Aircraft / Mechanical & Structural Applications / Seals; Aircraft / Mechanical & Structural Applications / Stock Shapes for Prototyping

Applications: Aircraft Applications; Electrical/Electronic Applications; Metal Replacement; Seals

Features: Chemical Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³ASTM D792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Viscosity 450 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
450 cP
@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.18 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.012 - 0.014 cm/cm
@Thickness 3.18 mm
0.012 - 0.014 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 380 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 105105ASTM D785
Tensile Strength 191 MPa27700 psi50 mm/min; ASTM D638
Tensile Strength, Yield 188 MPa
@Thickness 5.00 mm
27300 psi
@Thickness 0.197 in
Type 1A, 5 mm/min; ISO 527-2
Elongation at Break 1.8 %1.8 %5.0 mm/min; ASTM D638
 1.8 %1.8 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 15.1 GPa2190 ksi5.0 mm/min; ASTM D638
 16.7 GPa2420 ksi1 mm/min, Type 1A; ISO 527-2
Flexural Strength 250 MPa36300 psiISO 178
 54.0 MPa
@Temperature 250 °C
7830 psi
@Temperature 482 °F
ASTM D790
 253 MPa
@Temperature 23.0 °C
36700 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus 14.8 GPa2150 ksiASTM D790
 15.4 GPa2230 ksiISO 178
Compressive Strength 182 MPa26400 psiASTM D695
Shear Strength 89.0 MPa12900 psiASTM D732
Izod Impact, Notched 0.530 J/cm0.993 ft-lb/inASTM D256
Izod Impact, Unnotched 5.90 J/cm11.1 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 8.50 kJ/m²4.04 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 41.0 kJ/m²19.5 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.80e+17 ohm-cm1.80e+17 ohm-cmASTM D257
Surface Resistance >= 1.90e+17 ohm>= 1.90e+17 ohmASTM D257
Dielectric Constant  3.66
@Frequency 1e+6 Hz
3.66
@Frequency 1e+6 Hz
ASTM D150
 3.68
@Frequency 60 Hz
3.68
@Frequency 60 Hz
ASTM D150
 3.69
@Frequency 1000 Hz
3.69
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm483 kV/inASTM D149
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 0.0020
@Frequency 60 Hz
0.0020
@Frequency 60 Hz
ASTM D150
 0.0030
@Frequency 1e+6 Hz
0.0030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
Specific Heat Capacity  1.26 J/g-°C
@Temperature 50.0 °C
0.301 BTU/lb-°F
@Temperature 122 °F
ASTM C351
 1.62 J/g-°C
@Temperature 200 °C
0.387 BTU/lb-°F
@Temperature 392 °F
ASTM C351
Thermal Conductivity 0.310 W/m-K2.15 BTU-in/hr-ft²-°FASTM C177
Melting Point 345 °C653 °FPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 285 °C545 °FAnnealed; ASTM D648
Glass Transition Temp, Tg 150 °C302 °FDSC
Flammability, UL94  V-1
@Thickness 0.800 mm
V-1
@Thickness 0.0315 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 370 - 395 °C698 - 743 °FInjection
Mold Temperature 175 - 210 °C347 - 410 °F
Drying Temperature 150 - 175 °C
@Time 9000 - 14400 sec
302 - 347 °F
@Time 2.50 - 4.00 hour
Back Pressure 0.138 - 0.345 MPa20.0 - 50.0 psi
Screw Speed 75 rpm75 rpm
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw Compression Ratio2.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4158 / 279958

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.