MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mitsubishi Iupiace® TX903B m-Polyphenylene Ether (m-PPE)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Impact Grade

Material Notes: Anticreep high impact. Filler reinforced grade. Iupiace is a polymer alloy made by modifying PPE with high impact polystyrene (HIPS), nylon-6 or nylon-66. Usability in a wide range of temperatures (-40 to 160). Higher rigidity, impact strength and fatigue resistance. Excellent insulation properties, low dielectric constant and low dielectric dissipation factor. Excellent dimensional stability with low water absorption. Flame retardance and excellent self-extinguishing properties. Low density. Low shrinkage rate, ensuring quality precision parts. Good mold release, easy flow properties and a wide range of stock temperatures.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Water Absorption 0.060 %
@Temperature 23.0 °C
0.060 %
@Temperature 73.4 °F
Immersion
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 300 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 572 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiISO-527-1,2
Elongation at Break 40 %40 %ISO 527-1,2
Tensile Modulus 2.70 GPa392 ksiISO 527-1,2
Flexural Strength 100 MPa14500 psiISO 178
Flexural Modulus 2.70 GPa392 ksiISO 178
Charpy Impact Unnotched NBNBISO 179-1,2
Charpy Impact, Notched 3.20 J/cm²15.2 ft-lb/in²ISO 179-1,2
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °F
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FISO 75-1,2
Minimum Service Temperature, Air -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITSU9130 / 191803

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.