MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

96% Alumina, thick-film, as fired
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Key Words: aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.90 g/cc0.141 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  1.00e+6 ohm-cm
@Temperature 1000 °C
1.00e+6 ohm-cm
@Temperature 1830 °F
 4.00e+7 ohm-cm
@Temperature 700 °C
4.00e+7 ohm-cm
@Temperature 1290 °F
 5.00e+10 ohm-cm
@Temperature 300 °C
5.00e+10 ohm-cm
@Temperature 572 °F
 1.00e+14 ohm-cm
@Temperature 25.0 °C
1.00e+14 ohm-cm
@Temperature 77.0 °F
Dielectric Constant  9.5
@Frequency 1000 Hz
9.5
@Frequency 1000 Hz
 9.5
@Frequency 1e+6 Hz
9.5
@Frequency 1e+6 Hz
 9.5
@Frequency 1e+8 Hz
9.5
@Frequency 1e+8 Hz
Dissipation Factor  0.00040
@Frequency 1e+8 Hz
0.00040
@Frequency 1e+8 Hz
 0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
 0.0014
@Frequency 1e+6 Hz
0.0014
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  6.30 µm/m-°C
@Temperature 20.0 - 200 °C
3.50 µin/in-°F
@Temperature 68.0 - 392 °F
 7.10 µm/m-°C
@Temperature 20.0 - 500 °C
3.94 µin/in-°F
@Temperature 68.0 - 932 °F
 8.00 µm/m-°C
@Temperature 20.0 - 1000 °C
4.44 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 26.0 W/m-K180 BTU-in/hr-ft²-°F
 12.0 W/m-K
@Temperature 200 °C
83.3 BTU-in/hr-ft²-°F
@Temperature 392 °F
 20.0 W/m-K
@Temperature 100 °C
139 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 96 %96 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
92% Alumina, opaque
95% Alumina, vitreous body
85% Alumina, vitreous body
99.5% Alumina, vitreous body

BA2A / 135

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.