MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Bormed HE7541-PH is a bimodal, natural, high-density polyethylene produced by the Borstar PE technology. Bormed HE7541-PH combines low volatiles with high Environmental Stress Crack Resistance (ESCR) and superior flow properties as well as good impact strength and toughness even at low temperatures.

Bormed HE7541-PH is recommended for injection molding of caps and closures, pharmaceutical and diagnostic packaging, and IBM containers.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ISO 1183
ESCR 10% Igepal® >= 40 hour>= 40 hourASTM D1693
Linear Mold Shrinkage 0.020 cm/cm0.020 in/in
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ISO 868
Tensile Strength, Yield 22.0 MPa3190 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 10 %10 %At 50 mm/min; ISO 527-2
Tensile Modulus 0.850 GPa123 ksiAt 1 mm/min; ISO 527-2
Tensile Impact Strength 80.0 kJ/m²38.1 ft-lb/in²ISO 8256/A1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C149 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 250 °C374 - 482 °F
Mold Temperature 10.0 - 40.0 °C50.0 - 104 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
Borealis Bormed™ HE9621-PH HDPE for Healthcare Applications
Borealis MG7547S Polyethylene
LyondellBasell Alathon® M6138 High Density Polyethylene

PBOREA072 / 27379

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.