MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Tungsten, W, (drawn wire)
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy; Pure Element

Material Notes: Drawn wire applies only to tensile and hardness values; other property values are typical of tungsten.

Tungsten is a very dense, hard, temperature/corrosion-resistant metal. It is expensive so finds niche rather than large scale structural applications. Some example uses are rocket nozzles, nuclear and medical radiation shielding for x-ray and radiation therapy shields and industrial applications, aircraft and helicopter rotor balance weights, instrument balance weights, weights for sport equipment, tool damping cutter bars, and high voltage contacts.

Key Words: Wolfram, W
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 19.3 g/cc0.697 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 183.84183.841995
Atomic Number 7474
Thermal Neutron Cross Section 19.2 barns/atom19.2 barns/atom
X-ray Absorption Edge 0.17837 Å0.17837 ÅK
 1.02497 Å1.02497 ÅLI
 1.07436 Å1.07436 ÅLII
 1.21529 Å1.21529 ÅLIII
Electrode Potential 4.5 V4.5 V
Electronegativity 1.71.7Pauling
Ionic Radius 0.620 Å0.620 ÅCrystal Ionic Radius for Valence +6
 0.700 Å0.700 ÅCrystal Ionic Radius for Valence +4
Electrochemical Equivalent 3.43 g/A/h3.43 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 444444Converted from Vickers for 3000 kg load/10 mm ball Brinell test. Drawn and annealed.
Hardness, Knoop 505505Estimated from Vickers.
Hardness, Rockwell A 7474Converted from Vickers. Drawn and annealed.
Hardness, Rockwell C 4747Converted from Vickers. Drawn and annealed.
Hardness, Vickers 480480Drawn and annealed.
Tensile Strength, Yield 450 MPa65300 psi
Modulus of Elasticity 400 GPa58000 ksi
Poissons Ratio 0.280.28
Shear Modulus 156 GPa22600 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000565 ohm-cm0.00000565 ohm-cm
Magnetic Susceptibility 3.3e-73.3e-7cgs/g
Critical Magnetic Field Strength, Oersted 1.12 - 1.181.12 - 1.18
Critical Superconducting Temperature 0.0149 - 0.0159 K0.0149 - 0.0159 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 184.2 J/g79.24 BTU/lb
CTE, linear 4.40 µm/m-°C
@Temperature 20.0 - 100 °C
2.44 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.134 J/g-°C0.0320 BTU/lb-°F
Thermal Conductivity 163.3 W/m-K1133 BTU-in/hr-ft²-°F
Melting Point 3370 °C6100 °F
Boiling Point 5555 °C10030 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.15
@Temperature 100 °C
0.15
@Temperature 212 °F
unoxidized, total
 
Component Elements PropertiesMetricEnglishComments
Tungsten, W 100 %100 %
 
Descriptive Properties
CAS Number7440-33-7

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten, W
Copper, Cu; Annealed
304 Stainless Steel (UNS S30400); Cold Finished Wire
Copper, Cu; Cold-Worked
Tungsten Carbide, WC

AMEW001 / 127

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.