Celanese ZENITE 5145L LCP, 45% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Liquid Crystal Polymer (LCP)
;
Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
Material Notes:
Zenite« 5145L is a 45% glass fiber reinforced and toughened liquid crystal polymer for injection molding. It has improved toughness.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.75
g/cc
0.0632
lb/in³
ISO 1183
Density of Compound
1.48
g/cc
0.0535
lb/in³
Linear Mold Shrinkage, Flow
0.00090
cm/cm
0.00090
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0050
cm/cm
0.0050
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
115
MPa
16700
psi
5mm/min; ISO 527-2/1A
Elongation at Break
3.1 %
3.1 %
5mm/min; ISO 527-2/1A
Tensile Modulus
15.0
GPa
2180
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
190
MPa
27600
psi
ISO 178
Flexural Modulus
11.0
GPa
1600
ksi
ISO 178
Compressive Strength
71.0
MPa
10300
psi
ISO 604
21.3
MPa
@Strain 1 %
3090
psi
@Strain 1 %
ISO 604
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
1.00e+15
ohm
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
45.0
kV/mm
1140
kV/in
IEC 60243-1
Dissipation Factor
0.018
@Frequency 1e+6 Hz
0.018
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
175
V
175
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
7.00
µm/m-°C
3.89
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
60.0
µm/m-°C
33.3
µin/in-°F
ISO 11359-2
Specific Heat Capacity
1.50
J/g-°C
0.359
BTU/lb-°F
Thermal Conductivity
0.350
W/m-K
2.43
BTU-in/hr-ft²-°F
Melting Point
319
°C
606
°F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi)
290
°C
554
°F
ISO 75-1, -2
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Oxygen Index
33 %
33 %
ISO 4589
Processing Properties
Metric
English
Comments
Processing Temperature
80.0
-
120
°C
176
-
248
°F
cavity
Feed Temperature
40.0
-
60.0
°C
104
-
140
°F
Zone 1
320
-
330
°C
608
-
626
°F
Zone 2
335
-
345
°C
635
-
653
°F
Zone 3
335
-
345
°C
635
-
653
°F
Zone 4
335
-
345
°C
635
-
653
°F
Die Temperature
335
-
345
°C
635
-
653
°F
Melt Temperature
325
-
345
°C
617
-
653
°F
Ejection Temperature
265
°C
509
°F
Drying Temperature
>=
150
°C
>=
302
°F
Dry Time
3.00
hour
3.00
hour
Moisture Content
<= 0.010 %
<= 0.010 %
Injection Pressure
50.0
-
150
MPa
7250
-
21800
psi
Hold Pressure
50.0
-
150
MPa
7250
-
21800
psi
Back Pressure
<=
3.00
MPa
<=
435
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Vectra® C550 Liquid Crystal Polymer (LCP), 50% Mineral Filled
Celanese ZENITE 6635 LCP, 40% Mineral / Glass Reinforced (Extended Stress-Strain Tabular Data)
Celanese VECTRA E130i LCP, 30% Glass Reinforced
Dow Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
PHCQ535 / 178990
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.