MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Cancarb Thermax® Floform N990 Ultra-Pure Medium Thermal Carbon Black
Categories: Carbon; Carbon Black; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Thermal carbon black, often referred to as MT black, is unique in several ways. Along the carbon black spectrum, it has the largest particle size and among the lowest degrees of particle aggregation or structure. Since it is derived from natural gas, it is also one of the purest forms of carbon available on an industrial scale. Examples of its uses include applications in rubber, metallurgy, plastics, insulation, concrete and graphite, to name only a few.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oil Absorption 44 %44 %ml/100g; ASTM D2414
Particle Mesh Size 325 Mesh325 MeshSieve Residue = 20ppm; ASTM D1514
 325 Mesh325 MeshMagnetic Residue = 5ppm; ASTM D1514
pH 4.0 - 8.04.0 - 8.0ASTM D1512
Specific Surface Area 7.0 - 12 m²/g7.0 - 12 m²/gNitrogen; ASTM D6556
Ash 0.020 %0.020 %ASTM D1506
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 0.0060 %0.0060 %
 
Descriptive Properties
Fines Content (%)8ASTM D1508
Heat Loss (%)0.1ASTM D1509
Pellet Hardness (14x18 mesh) (grams)30ASTM D5230; Average
 50ASTM D5230; High
Toluene Extract (%)0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cancarb Thermax® Floform N990 Medium Thermal Carbon Black
Cancarb Thermax® Powder N908 Stainless Medium Carbon Black
Graphite, Carbon, C
Cancarb Thermax® Powder N991 Ultra-Pure Medium Thermal Carbon Black
Cancarb Thermax® Floform N907 Stainless Medium Carbon Black

CCAN005 / 79042

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.