Physical Properties | Metric | English | Comments |
---|
Density | 0.602 g/cc @Temperature 1000 °C | 0.0217 lb/in³ @Temperature 1830 °F |
| 0.653 g/cc @Temperature 800 °C | 0.0236 lb/in³ @Temperature 1470 °F |
| 0.702 g/cc @Temperature 600 °C | 0.0254 lb/in³ @Temperature 1110 °F |
| 0.751 g/cc @Temperature 400 °C | 0.0271 lb/in³ @Temperature 752 °F |
| 0.774 g/cc @Temperature 300 °C | 0.0280 lb/in³ @Temperature 572 °F |
| 0.797 g/cc @Temperature 200 °C | 0.0288 lb/in³ @Temperature 392 °F |
| 0.820 g/cc @Temperature 100 °C | 0.0296 lb/in³ @Temperature 212 °F |
| 0.855 g/cc @Temperature 20.0 °C | 0.0309 lb/in³ @Temperature 68.0 °F |
| 0.873 g/cc @Temperature -73.0 °C | 0.0315 lb/in³ @Temperature -99.4 °F |
| 0.894 g/cc @Temperature -173 °C | 0.0323 lb/in³ @Temperature -279 °F |
| 0.909 g/cc @Temperature -270 °C | 0.0328 lb/in³ @Temperature -454 °F |
Vapor Pressure | 0.150 bar @Temperature 590 °C | 113 torr @Temperature 1090 °F |
| 0.500 bar @Temperature 710 °C | 375 torr @Temperature 1310 °F |
| 1.00 bar @Temperature 770 °C | 750 torr @Temperature 1420 °F |
| 2.00 bar @Temperature 850 °C | 1500 torr @Temperature 1560 °F |
| 5.00 bar @Temperature 950 °C | 3750 torr @Temperature 1740 °F |
| 10.0 bar @Temperature 1110 °C | 7500 torr @Temperature 2030 °F |
| 20.0 bar @Temperature 1240 °C | 15000 torr @Temperature 2260 °F |
| 40.0 bar @Temperature 1420 °C | 30000 torr @Temperature 2590 °F |
|
Chemical Properties | Metric | English | Comments |
---|
Atomic Mass | 39.0983 | 39.0983 |
Atomic Number | 19 | 19 |
Thermal Neutron Cross Section | 2.7 barns/atom | 2.7 barns/atom |
X-ray Absorption Edge | 3.43645 Å | 3.43645 Å |
| 36.352 Å | 36.352 Å |
| 42.02 Å | 42.02 Å |
| 42.452 Å | 42.452 Å |
Critical Temperature | 1950 °C | 3540 °F |
Electrode Potential | -2.92 V | -2.92 V |
Electronegativity | 0.82 | 0.82 |
Ionic Radius | 1.33 Å | 1.33 Å |
Electrochemical Equivalent | 1.46 g/A/h | 1.46 g/A/h |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 0.00000649 ohm-cm @Temperature 0.000 °C | 0.00000649 ohm-cm @Temperature 32.0 °F |
| 0.00000720 ohm-cm @Temperature 20.0 °C | 0.00000720 ohm-cm @Temperature 68.0 °F |
| 0.00000922 ohm-cm @Temperature 63.0 °C | 0.00000922 ohm-cm @Temperature 145 °F |
| 0.00001395 ohm-cm @Temperature 63.0 °C | 0.00001395 ohm-cm @Temperature 145 °F |
| 0.00001464 ohm-cm @Temperature 77.0 °C | 0.00001464 ohm-cm @Temperature 171 °F |
Magnetic Susceptibility | 5.2e-7 | 5.2e-7 |
|
Thermal Properties | Metric | English | Comments |
---|
Heat of Fusion | 61.55 J/g | 26.48 BTU/lb |
Heat of Vaporization | 2077 J/g | 893.5 BTU/lb |
CTE, linear | 83.0 µm/m-°C @Temperature 20.0 - 100 °C | 46.1 µin/in-°F @Temperature 68.0 - 212 °F |
Specific Heat Capacity | 0.532 J/g-°C | 0.127 BTU/lb-°F |
| 0.724 J/g-°C | 0.173 BTU/lb-°F |
Thermal Conductivity | 99.2 W/m-K | 688 BTU-in/hr-ft²-°F |
Melting Point | 63.25 °C | 145.9 °F |
Boiling Point | 759 °C | 1400 °F |
Heat of Formation | 0.000 kJ/mol | 0.000 kJ/mol |
| 89.0 kJ/mol | 89.0 kJ/mol |
|
Component Elements Properties | Metric | English | Comments |
---|
Potassium, K | 100 % | 100 % |
|
Descriptive Properties |
---|
CAS Number | 7440-09-7 |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.