MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company ESD 3282 Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber - Electrically Conductive
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE, with Glass or Carbon Fiber Filler

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.72 g/cc1.72 g/ccASTM D 792
Additive Loading 15 %15 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 41.4 MPa6000 psiASTM D 638
Elongation at Break 5.0 - 10 %5.0 - 10 %ASTM D 638
Tensile Modulus 10.3 GPa1500 ksiASTM D 638
Flexural Strength 64.1 MPa9300 psiASTM D 790
Flexural Modulus 8.27 GPa1200 ksiASTM D 790
Izod Impact, Notched 4.27 J/cm
@Thickness 3.20 mm
8.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 8.01 J/cm
@Thickness 3.20 mm
15.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10000 ohm-cm<= 10000 ohm-cmASTM D 257
Surface Resistance <= 1.00e+6 ohm<= 1.00e+6 ohmESD STM11.11
Surface Resistivity per Square <= 1.00e+7 ohm<= 1.00e+7 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secFTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C400 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 293 - 343 °C560 - 650 °F
Mold Temperature 65.6 - 149 °C150 - 300 °F
Drying Temperature 121 °C
@Time 7200 sec
250 °F
@Time 2.00 hour
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company ESD 3281 Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber - Static Dissipative
RTP Company RTP 3200 MG 20 Ethylene Tetrafluoroethylene (ETFE), Milled Glass
RTP Company RTP 3283  Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber 20%
RTP Company RTP 3281  Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber 10%
RTP Company RTP 3205  Ethylene Tetrafluoroethylene (ETFE) Glass Fiber 30%

PQZTA27542 / 171691

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.