MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Antistat/Conductive

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.14 - 1.53 g/cc0.0412 - 0.0553 lb/in³Average value: 1.31 g/cc Grade Count:33
Filler Content 5.00 - 20.0 %5.00 - 20.0 %Average value: 11.7 % Grade Count:3
Water Absorption 0.100 - 0.120 %0.100 - 0.120 %Average value: 0.105 % Grade Count:4
Additive Loading 6.00 - 20.0 %6.00 - 20.0 %Average value: 15.9 % Grade Count:7
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm0.00100 - 0.0200 in/inAverage value: 0.00563 cm/cm Grade Count:30
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 37.9 - 124 MPa5500 - 18000 psiAverage value: 67.6 MPa Grade Count:31
Elongation at Break 1.00 - 10.0 %1.00 - 10.0 %Average value: 5.66 % Grade Count:33
Modulus of Elasticity 1.72 - 12.4 GPa250 - 1800 ksiAverage value: 4.45 GPa Grade Count:30
Flexural Yield Strength 55.2 - 193 MPa8000 - 28000 psiAverage value: 110 MPa Grade Count:33
Flexural Modulus 1.72 - 11.0 GPa250 - 1600 ksiAverage value: 4.35 GPa Grade Count:33
Izod Impact, Notched 0.320 - 10.7 J/cm0.600 - 20.0 ft-lb/inAverage value: 1.56 J/cm Grade Count:33
Izod Impact, Unnotched 2.67 - 5340 J/cm5.00 - 10000 ft-lb/inAverage value: 6.34 J/cm Grade Count:32
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00 - 1.00e+11 ohm-cm1.00 - 1.00e+11 ohm-cmAverage value: 4.87e+9 ohm-cm Grade Count:32
Surface Resistance 1.00 - 1.00e+12 ohm1.00 - 1.00e+12 ohmAverage value: 3.44e+10 ohm Grade Count:33
Static Decay 0.100 - 2.00 sec0.100 - 2.00 secAverage value: 0.900 sec Grade Count:28
Shielding Effectiveness 35.0 - 106 dB35.0 - 106 dBAverage value: 76.1 dB Grade Count:15
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.8 - 124 °C172 - 255 °FAverage value: 108 °C Grade Count:15
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:19
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 - 293 °C420 - 560 °FAverage value: 255 °C Grade Count:31
Mold Temperature 37.8 - 98.9 °C100 - 210 °FAverage value: 71.7 °C Grade Count:31
Drying Temperature 79.4 - 120 °C175 - 248 °FAverage value: 93.3 °C Grade Count:31
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.0320 % Grade Count:30
Dew Point -28.9 - -17.8 °C-20.0 - 0.000 °FAverage value: -28.5 °C Grade Count:29
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
Overview of materials for PC/ABS + Stainless Steel
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled

O1174a / 89064

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.