System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.
The ComAlloy product line has been integrated into the A Schulman product line.
Key Words:
Poly(Acrylonitrile Butadiene Styrene); ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.13
g/cc
0.0408
lb/in³
Linear Mold Shrinkage
0.0030
cm/cm
0.0030
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
112
112
ASTM D785
Tensile Strength, Ultimate
43.0
MPa
6240
psi
ASTM D638
Elongation at Break
2.0 %
2.0 %
ASTM D638
Flexural Strength
57.0
MPa
8270
psi
ASTM D790
Flexural Modulus
4.00
GPa
580
ksi
ASTM D790
Izod Impact, Unnotched
0.600
J/cm
1.12
ft-lb/in
ASTM D256
Electrical Properties
Metric
English
Comments
Electrical Resistivity
100
-
1000
ohm-cm
100
-
1000
ohm-cm
Surface Resistance
1000
-
10000
ohm
1000
-
10000
ohm
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
100
°C
212
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
92.0
°C
198
°F
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Asahi Kasei Stylac™ IC24 ABS Polymer, Electrically Conductive
Asahi Kasei Stylac™ IC10N ABS Polymer, Electrically Conductive
EMS-Grivory Grilamid® LC-15H black PA12-CF15
Covestro Bayblend® T50 XF Polycarbonate + ABS
Carlisle 201LD Carbon-Carbon Composite
PASH58 / 24951
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.