MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Arya Sasol LFI 2130 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description: LFI2130 is a high molecular weight, low density polyethylene for producing heavy-duty packaging films for applications like shrink hoods. It contains no slip agent and antiblock additives. It gives outstanding strength and toughness, draw down ability and very good biaxial shrink properties. LFI2130 has been manufactured under SABTEC licensed technology.

Application: Blown film extrusion, heavy duty packaging film shrink hoods, industrial sacks, carrier bag and liners

Forms: Pellets

Attribute: Good strength and toughness, very good melt strength.

No Additives

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ISO 1183
Thickness 45.0 - 150 microns1.77 - 5.91 mil
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiISO 527-1,3
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiISO 527-1,3
Film Elongation at Break, MD >= 350 %>= 350 %ISO 527-1,3
Film Elongation at Break, TD >= 500 %>= 500 %ISO 527-1,3
Modulus of Elasticity 0.140 GPa20.3 ksiMD; ISO 527-1,3
 0.150 GPa21.8 ksiTD; ISO 527-1,3
Coefficient of Friction 0.700.70ASTM D1894
Tear Strength 20.0 kN/m114 pliMD; ISO 6383-2
 45.0 kN/m257 pliTD; ISO 6383-2
Dart Drop Total Energy 31.0 J/cm0.0581 ft-lb/milASTM D4272
Film Tensile Strength at Break, MD 22.0 MPa3190 psiISO 527-1,3
Film Tensile Strength at Break, TD 24.0 MPa3480 psiISO 527-1,3
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003 A
Gloss 55 %55 %[GU], 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 185 - 210 °C365 - 410 °FExtruder temperature profile
Blow-up Ratio (BUR) 2.0 - 4.02.0 - 4.0
 
Descriptive Properties
Blocking<5 gASTM D3354
Clarity50 mVSABTEC method
Re-blocking20 gSABTEC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARYA000 / 250454

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.