MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chosun Refractories SCX-90 I Special SiC Castable
Categories: Ceramic; Carbide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  39.2 MPa
@Treatment Temp. 110 °C,
Time 86400 sec
5690 psi
@Treatment Temp. 230 °F,
Time 24.0 hour
Cold Crushing Strength
 98.1 MPa
@Treatment Temp. 1400 °C,
Time 10800 sec
14200 psi
@Treatment Temp. 2550 °F,
Time 3.00 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.00 %
@Temperature 110 °C,
Time 86400 sec
0.00 %
@Temperature 230 °F,
Time 24.0 hour
 
Component Elements PropertiesMetricEnglishComments
SiC 90 %90 %
 
Descriptive Properties
Installation MethodCasting, Spray
Material Required for Estimating (kg/m3)2,600
Water Required for Casting(%)6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Silicon Carbide, CVD
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%)
Ceradyne Ceralloy® 13740Y AlN-SiC
Ceradyne CeraTrex™ 146-12E Silicon Carbide

CCHOS194 / 124138

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.