MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Goodfellow Reaction Bonded Silicon Carbide SiC
Categories: Ceramic; Carbide

Material Notes: Produced by silicon infiltration into a pre-formed silicon carbide/carbon powder green body, which is subsequently fired. This gives rise to around 10% free silicon, which fills the pores. The resulting microstructure has low porosity and a very fine grain. Shaping is normally carried out before firing, but the fired compact can be diamond ground to around 0.01 mm tolerance. Iit is difficult to machine after firing. The material has high strength up to 1350°C which results in its use as high temperature gas turbine components. The high hardness (harder than tungsten carbide) means that it is used extensively for bearings and seals. The high thermal conductivity combined with low thermal expansion leads to good thermal shock resistance. RBSC can tolerate a wider range of acids and alkalis than either tungsten carbide or alumina. Its oxidation resistance helps to give long service life in furnace applications.

Information provided by Goodfellow.

Key Words: REFEL F®; RBSC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.10 g/cc0.112 lb/in³
Porosity 0.00 %0.00 %Apparent
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 2000 - 35002000 - 3500kgf/mm²
Tensile Modulus 410 GPa59500 ksi
Compressive Strength 2000 - 3500 MPa290000 - 508000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 1000 ohm-cm100 - 1000 ohm-cm
Dielectric Constant 1010
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.30 - 4.60 µm/m-°C
@Temperature 20.0 - 1000 °C
2.39 - 2.56 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°F
Thermal Conductivity 150 - 200 W/m-K1040 - 1390 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1350 °C2460 °F
 
Component Elements PropertiesMetricEnglishComments
SiC 100 %100 %
 
Descriptive Properties
Chemical Resistance - AlkalisFair
Chemical Resistance - Concentrated AcidsGood
Chemical Resistance - Dilute AcidsGood
Chemical Resistance - HalogensFair
Chemical Resistance - MetalsFair

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Hot Pressed Silicon Carbide SiC
Schunk CarSIK NT Silicon Carbide
Inhance Fluoro-Seal INHANCE® Ti-9000 Titanium Carbide
Morgan Advanced Ceramics Performance SiC CVD SiC chemical vapor desposition Silicon Carbide
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB

CGOODF245 / 197408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.