MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Vamac® GLS Ethylene Methacrylate (AEM)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Vamac® GLS is a terpolymer of ethylene, methylacrylate, and a cure site monomer cured using an diamine-based vulcanization system. Compared with Vamac® G, Vamac® GLS offers significantly improved resistance to oil swell and chemicals such as diesel fuel. Vamac® GLS elastomer contains a small amount of processing aid. Storage stability is excellent.

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Volatiles <= 0.40 %<= 0.40 %EN 1400 / EN 14350-2
Mooney Viscosity  18.5
@Temperature 100 °C
18.5
@Temperature 212 °F
ML 1+4; ISO 289-1-2
 40
@Temperature 100 °C
40
@Temperature 212 °F
ML 1+4, Compound; ISO 289-1-2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6868ASTM D 2240
Tensile Stress at Strain 6.40 MPa
@Strain 100 %
928 psi
@Strain 100 %
ISO 527-1/-2
Tear Strength 34.0 kN/m194 pliparallel; ISO 34-1
Compression Set  20 %
@Temperature 150 °C,
Time 252000 sec
20 %
@Temperature 302 °F,
Time 70.0 hour
ISO 815
 28 %
@Temperature 150 °C,
Time 605000 sec
28 %
@Temperature 302 °F,
Time 168 hour
ASTM D 395B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 175 °C347 °FDuPont proprietary test
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 °C
@Time 14400 sec
347 °F
@Time 4.00 hour
Cure Time 5.00 min
@Temperature 175 °C
0.0833 hour
@Temperature 347 °F
 
Descriptive Properties
Colorclear to light yellow translucent
Part Marking Code>AEM<ISO 11469
Polymer(AEM)
Resin IdentificationAEMISO 1043
Scorch, Mooney viscosity> 15MS at 121°C; ISO 289-1-2
Scorch, time to 10 unit rise10MS at 121°C; ISO 289-1-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4609 / 265819

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.