MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALCOM® POM 770/1.1 CF20 POM, 20% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Carbon Fiber Filled

Material Notes: Base Polymer: Polyoxymethylene Copolymer

Filler/Additive System: 20% Carbon Fibers

Special Features: Electrically conductive, reduced surface resistivity, high stiffness

Market Segment: Automotive, Machinery

Application Area: Various

Typical Application: Functional components, bearings

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Time 86400 sec
0.0070 - 0.0090 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Time 86400 sec
0.0080 - 0.010 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psiISO 527
Elongation at Break 0.60 %0.60 %ISO 527
Tensile Modulus 14.5 GPa2100 ksiISO 527
Flexural Strength 100 MPa14500 psiISO 178
Flexural Modulus 11.5 GPa1670 ksiISO 178
Charpy Impact Unnotched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 170 °C338 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FISO 75-1/-2
Vicat Softening Point 156 °C313 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °FInjection molding
Mold Temperature 60.0 - 120 °C140 - 248 °FInjection molding
Drying Temperature  100 - 110 °C
@Time 7200 - 10800 sec
212 - 230 °F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
 100 - 110 °C
@Time 10800 - 18000 sec
212 - 230 °F
@Time 3.00 - 5.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerPolyoxymethylene Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accucomp Polyacetal (POM) ACE091L High Viscosity
Asahi Kasei TENAC™-C CF454 Copolymer Acetal (POM), Medium Viscosity, Carbon Fiber Reinforced
Aclo Accucomp Polyacetal (POM) ACE093L Low Viscosity
Barlog Plastics KEBAFORM C 520.0 POM Copolymer unreinforced
EPICHEM Epiryl PPO V0 Polyphenylene oxide

PALBIS8570 / 242629

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.