MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

GEHR Plastics PVC-C®
Categories: Polymer; Thermoplastic; Vinyl (PVC); Chlorinated PVC (CPVC)

Material Notes: PVC-C has high rigidity, strength, and hardness at increased temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Water Absorption at Saturation 0.50 %0.50 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ISO 868
Ball Indentation Hardness 150 MPa21800 psiISO 2039
Tensile Strength at Break 33.9 MPa4910 psiASTM D638
 80.0 MPa11600 psiISO 527
Tensile Strength, Yield 48.9 MPa7090 psiASTM D638
 49.0 MPa7110 psiISO 527
Elongation at Break 15 %15 %ISO 527
 23 %23 %ASTM D638
Elongation at Yield 2.3 %2.3 %ASTM D638
 5.0 %5.0 %ISO 527
Modulus of Elasticity 2.56 GPa372 ksiASTM D638
 2.57 GPa373 ksiISO 527
Flexural Strength 73.1 MPa10600 psiASTM D638
 76.0 MPa11000 psiISO 178
Izod Impact, Notched 0.694 J/cm1.30 ft-lb/inASTM D256
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 2.70 J/cm²12.8 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm1020 kV/inIEC 60243-1
Dielectric Loss Index 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VKB; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FISO 11359
 103 µm/m-°C57.0 µin/in-°FASTM D696
Thermal Conductivity 0.140 W/m-K
@Temperature 20.0 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
ISO 22007-4
Melting Point 110 °C230 °FDIN EN ISO 3146
Maximum Service Temperature, Air 85.0 °C185 °FUL 746B
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FISO 75
 105 °C221 °FASTM D648
Vicat Softening Point 114 °C237 °FVST/B/50; ISO 306
Minimum Service Temperature, Air -15.0 °C5.00 °FUL 746B
Glass Transition Temp, Tg 110 °C230 °FDIN EN ISO 3146
Flammability, UL94 V-0V-0UL 94
Oxygen Index 65 %65 %ASTM D2863
 
Compliance PropertiesMetricEnglishComments
FDA YesYesPhysiological indifference; NSF-61 ,FDA
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistancelimited
Bondabilityyes
Chemical ResistanceDIN 8061
CKW Resistanceno
Colorlight grey
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistancelimited
Physiological indifferenceno, EEC
Resistance Against Hot Waterlimited
UV Stabilizationno

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet
Overview of materials for Chlorinated PVC (CPVC)
Vycom Corzan® CPVC Chlorinated PVC
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding

PGEHR004 / 79841

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.