MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema LOTRYL® Bestpeel 2407 Copolymer Ethylene - Methyl Acrylate
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: LOTRYL® Bestpeel 2407 is a ready-to-use thermoplastic composition designed to make peelable heat seal layers onto various substrates. The base resin is a random copolymer of ethylene and methyl acrylate, polymerized by high-pressure process in autoclave reactor. Modification is introduced to ensure the best processability in the different film technologies, and the suitable properties in heat sealing and peeling.

General properties

The chemical structure of LOTRYL® Bestpeel 2407 combines the properties and processability of an autoclaveethylenic backbone together with the softness and polarity brought by acrylic ester groups. Composition has been optimized in order that

  • LOTRYL® Bestpeel 2407 is highly compatible with polyethylene, leading to perfect adhesion in coextrusion with polyethylene and with most of ethylene copolymers.
  • The amount of methyl acrylate comonomer as well as its uniform distribution give optimum compatibility with PP, PS, PET and PVC, which leads to a very balanced performance between strength of sealing and ease of peeling.

ApplicationsLOTRYL® Bestpeel 2407 is used as top layer of laminates in order to provide the functions of heat sealability onto various substrates like PP, PS, PET and PVC, and easy opening by interfacial peeling. LOTRYL® Bestpeel 2407 is easily processed using the technologies of coextrusion coating, cast film coextrusion, blown film coextrusion or sheet coextrusion, to produce multilayers that can be used as lids, either directly or after lamination with other films.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc
@Temperature 23.0 °C
0.0340 lb/in³
@Temperature 73.4 °F
ISO 1183
Methyl Acrylate Content 24 %24 %FTIR (internal)
Melt Index of Compound 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7979ISO 868
Hardness, Shore D 2222ISO 868
Elongation at Break 750 %750 %ASTM D638
Flexural Modulus 0.0140 GPa2.03 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 69.0 °C156 °FDSC
Vicat Softening Point <= 40.0 °C
@Load 1.02 kg
<= 104 °F
@Load 2.25 lb
ASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 170 °C>= 338 °Fin blown film extrusion
 <= 310 °C<= 590 °Fin extrusion coating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema LOTRYL® 16 MA 003 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate

PARKG213 / 80074

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.