MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AdvanSix Aegis® CSD High Barrier Nylon  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
Oxygen Transmission 0.236 cc-mm/m²-24hr-atm0.600 cc-mil/100 in²-24hr-atm80% RH, 23°C, cast film
Carbon Dioxide Transmission 0.472 cc-mm/m²-24hr-atm1.20 cc-mil/100 in²-24hr-atm80% RH, 23°C, oriented film
Melt Index of Compound  14 g/10 min
@Load 2.16 kg,
Temperature 260 °C
14 g/10 min
@Load 4.76 lb,
Temperature 500 °F
 24 g/10 min
@Load 2.16 kg,
Temperature 280 °C
24 g/10 min
@Load 4.76 lb,
Temperature 536 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 102 MPa14800 psioriented film
Tensile Strength, Yield 90.3 MPa13100 psioriented film, Yield Stress
Elongation at Break 42 %42 %oriented film
Elongation at Yield 4.0 %4.0 %oriented film
Secant Modulus 3.013 GPa437.0 ksioriented film
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 82.0 °C180 °FDSC method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 280 °C518 - 536 °F
Feed Temperature 25.0 °C77.0 °F
Nozzle Temperature 280 °C536 °F
Zone 1 260 °C500 °F
Zone 2 270 °C518 °F
Zone 3 270 °C518 °F
Zone 4 275 °C527 °F
Zone 5 280 °C536 °F
Melt Temperature 233 °C451 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALA02 / 23094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.